5083 in H116/H321 tempers for hull, deck and tank work. 0.5–4 mm coil supplied cut-to-size with EN 10204 3.1 MTC per batch.

2.66 g/cm³305 MPa0.5–4 mm2,650 mm wide

Product views

5083 mill-finish coils, yard stock, packing and tank applications.

×
5083 coil view 1
5083 coil view 1
×
5083 coil view 2
5083 coil view 2
×
5083 coil detail 1
5083 coil detail 1
×
5083 coil detail 2
5083 coil detail 2
Density2.66g/cm³ · ≈1/3 of steel
Tensile305MPa · H116 min
Thickness0.5–4mm coil
Width2,650mm · 3,000 on request
Length12,000mm cut-to-length

Other 5xxx grades we supply

Same marine family, different balance of strength, formability and service temperature.

Which temper do you need?

Pick the stabilised temper for the exposure and forming requirements of each part.

Hull default
H116

The default stabilised temper for hull and weather-deck plating.

  • 305 MPa tensile / 215 MPa proof min
  • ASTM G66 & G67 qualified
  • Splash zone & permanent immersion
H321

Thermally stabilised; specified interchangeably with H116 for primary structure.

  • Same minimum strength as H116
  • Lower-temperature stabilisation
  • Common in LNG secondary barrier
H111 / H112

For formed panels and non-critical structure where forming wins over as-welded strength.

  • 275–350 MPa tensile / 125 MPa proof min
  • Deep panels, cabins, interiors
  • O temper for bent parts

Where 5083 coil is used on board

5083 coil thickness starts at 0.5 mm; heavier sections carry primary loads.

Continuous forming

Coil-fed press brake and roll-forming lines for long production runs of panels and profiles.

0.5–4 mm

Deck & roof panels

Slit coil is decoiled and profiled into deck and roof panels for accommodation blocks.

0.8–2 mm

Tank liner coil

5083-H111 coil is used for welded tank liners and chine liners in series-built boats.

1–3 mm

Small craft series production

Consistent coil lot size helps maintain traceability across a batch of hulls.

1–3 mm

Why 5083 wins in marine service

Four numbers that decide the specification.

15–20%lighter than steel

Same section modulus, lower center of gravity and fuel burn.

ER5356matched weld filler

Compatible filler chemistry keeps joints corrosion-resistant without post-weld heat treatment.

EN 10204 3.1per-batch MTC

Mill test certificate issued by the producing mill and countersigned by our QC team.

65 °Cservice ceiling

For long-term service above this, 5454 is the usual alternative.

Real-world corrosion resistance

8-year atmospheric and splash-zone exposure data on Al–Mg 5xxx alloys.

Qingdao atmosphere
<0.4 μm/a
Xiamen splash zone
0.39 mm max pit
Qingdao atmosphereXiamen splash zone
  • Stabilised tempers: H116/H321 keep intergranular and exfoliation corrosion low in continuous immersion and splash zones.
  • Lot-release testing: ASTM G66 ASSET and G67 NAMLT confirm resistance to sensitisation before shipment.
  • Design matters: isolate aluminum from dissimilar metals, avoid standing water in crevices, and stay below the 65 °C long-term ceiling.

Actual rates depend on local water chemistry, design and maintenance.

5083 coil with heat and lot marking
5083 coil with heat and lot marking — traceable to the mill certificate.

5083 mechanical properties

Minimum / typical values per ASTM B209 / B928. Certified values are shown on the EN 10204 3.1 MTC supplied with each batch.

TemperTensile Rm (MPa)Proof Rp0.2 (MPa)Elongation A50 (%)Typical marine use
O270–345115–200≥16Deep-drawn and bent parts
H111275–350≥125≥14Formed panels, cabins, interiors
H112275–350≥125≥12Hot-rolled plate, non-critical structure
H116305 min≥215≥10Hull plating, splash zone, weather decks
H321305–385≥21510–12Hull plating, LNG secondary barrier

Plate above 40 mm thickness is rated at 285 MPa min tensile and 200 MPa min proof stress per ASTM B928.

5083 against the rest of the 5xxx family

Every grade below we supply. Choose on strength, forming and service temperature — not on habit.

AlloyMg content (%)Tensile Rm (MPa)Proof Rp0.2 (MPa)Marine corrosionBest used for
50834.0–4.9305–385≥215Excellent — G66/G67Hull, deck, LNG secondary barrier
50863.5–4.5275–345≥195ExcellentHull plating, fast craft, pressure vessels
57542.6–3.6215–275≥130Very goodSuperstructures, tanks, general fabrication
50522.2–2.8215–265≥160Very goodFuel tanks, panelling, ducting
54542.4–3.0240–290≥180Excellent at temperatureWarm service above 65 °C, chemical carriers
51824.0–5.0275–350≥130GoodTank bodies, stiffeners, reinforcement

Typical values for common marine tempers. Higher-magnesium grades give more strength but were designed for different forming limits — confirm the temper before substituting.

Marine standards & classification

Certification and testing that shipyard buyers actually ask for.

ASTM B928High-Mg marine sheet & plate
ASTM B209General aluminum sheet & plate
DNV NV-5083Rules Pt.2 Ch.2 Sec.10
EN 10204 3.1Mill test certificate
EN 485-2Dimensions & tolerances

How we supply 5083 coil

From producing mill to yard, with independent QC at each step.

Slit to width

Coil slit to your exact width, edge-dressed and recoiled for continuous forming lines.

Slitting

Sea-export packing

Wooden stillage, edge protection, waterproof film. Steel strapping for heavy plate.

Export

Per-batch certificate

EN 10204 3.1 MTC issued by the producing mill and countersigned by our QC team.

3.1 MTC

Frequently asked questions

Which 5083 temper do I need for hull plating?

H116 is specified for most hull and splash-zone plating. H321 is accepted interchangeably and is often chosen for thicker sections or when the order references a wider thickness range.

What thickness and width can you supply?

3–50 mm thickness, widths up to 2,650 mm (3,000 mm on request), cut-to-length up to 12,000 mm.

Is 5083 plate suitable for LNG tanks?

Yes. 5083 retains toughness at cryogenic temperatures and is widely used for LNG secondary barrier and storage-tank walls.

Can you supply cut-to-size plate, or only standard sizes?

We supply cut-to-size. Send us your nesting or finished dimensions, and we will quote against your spec rather than a fixed stock list.

Do you have classification society certification?

DNV certification is available with the order; other major classification societies can be requested. An EN 10204 3.1 MTC accompanies every batch.

What is the difference between 5083 plate and 5083 sheet?

Same alloy, different thickness ranges. Plate generally starts at 3 mm and is used for primary structure; sheet is thinner and is used for panels, decking and formed parts.

What filler wire should I use for welding 5083?

ER5183 for high-strength joints; ER5356 for general fabrication where a small strength mismatch is acceptable.

What certificate comes with each order?

An EN 10204 3.1 MTC per batch, issued by the producing mill and countersigned by our QC team after independent re-inspection.

Need a 5083 marine coil quotation?

Send grade, temper, thickness, width and quantity — we quote against current mill availability.

Request a quoteEmail info@aymetals.com
Grades supplied5083 · 5086 · 5754 · 5052 · 5454 · 5182
Thickness range0.5 – 4 mm
CertificateEN 10204 3.1 per batch
Cut-to-lengthUp to 12,000 mm

Delin Aluminum has supplied 5xxx marine plate and sheet for over 10 years. Material comes from mills holding DNV approval, with other major classification societies available on request.

Related resources